MATERIAL RECORD

430 Stainless Steel

A practical 430 stainless steel grade reference covering common designations, its ferritic family, typical uses and selection limits.

FerriticUNS S43000 EN 1.4016 JIS SUS430

COMMON DESIGNATIONS

Grade identifiers

UNSUnified Numbering System designation
S43000
ENEuropean standard number
1.4016
JISJapanese Industrial Standards designation
SUS430

These are commonly cited designation mappings. They do not establish one-to-one equivalence for every product form or specification; confirm the required standard and material certificate.

MATERIAL PROFILE

A common ferritic stainless sheet grade

430 is a ferritic stainless steel commonly referenced as UNS S43000 and EN 1.4016; JIS SUS430 is a common cross-reference. Outokumpu describes its 430/4016 product as a ferritic grade for mildly corrosive environments, particularly indoor use. Product form, surface condition and the applicable standard determine the delivered material properties.

GRADE COMPARISON / 01

How 304, 316L and 430 differ

Compare the alloy families and published chemistry ranges first. They help explain where each grade is commonly considered, but they do not replace a check against the service environment and the specified product standard.

Typical composition ranges (% by mass)

0 — 20%

Cr · Chromium Ni · Nickel Mo · Molybdenum

304

304 Stainless Steel

Austenitic

A widely used austenitic chromium-nickel grade for general-purpose applications that need formability and corrosion resistance.

304 Stainless SteelEach bar shows the listed minimum-to-maximum range on a shared scale from zero to twenty percent. A dash means no range is listed in that reference table; it does not mean the element is physically absent.05101520Cr17.5–19.5%Ni8–10.5%Mo
Chromium
17.5–19.5%
Nickel
8–10.5%
Molybdenum
Not listed in this table

Selection context

For chloride-rich or more aggressive corrosive service, assess 316/316L or another grade against the actual environment. Grade 304 is not a universal choice; this summary does not qualify material for a specific application.

316L

316L Stainless Steel

Austenitic · Mo alloyed

A low-carbon 316 grade with molybdenum, considered where more resistance to localized corrosion is needed than a basic 304 grade provides.

316L Stainless SteelEach bar shows the listed minimum-to-maximum range on a shared scale from zero to twenty percent. A dash means no range is listed in that reference table; it does not mean the element is physically absent.05101520Cr16–18%Ni10–14%Mo2–3%
Chromium
16–18%
Nickel
10–14%
Molybdenum
2–3%

Selection context

The low-carbon designation and molybdenum addition do not make 316L immune to corrosion. Temperature, chloride concentration, crevices, surface finish, fabrication and the governing standard all affect selection.

430

430 Stainless Steel

FerriticThis page

A ferritic chromium stainless steel commonly specified in sheet form for mildly corrosive and indoor applications.

430 Stainless SteelEach bar shows the listed minimum-to-maximum range on a shared scale from zero to twenty percent. A dash means no range is listed in that reference table; it does not mean the element is physically absent.05101520Cr16–18%NiMo
Chromium
16–18%
Nickel
Not listed in this table
Molybdenum
Not listed in this table

Selection context

430 belongs to the ferritic family, while 304 and 316L are austenitic. Check the service environment, fabrication route and required product standard before comparing or substituting grades.

Ranges follow the cited British Stainless Steel Association reference tables for these grade designations. A dash means that table lists no range, not zero content. Product-form standards can differ; verify the specification and mill certificate before ordering.

Composition references

British Stainless Steel Association

APPLICATION CONTEXT

Where it is commonly considered

Typical references include kitchen equipment, household appliances, sinks, elevators and other indoor equipment. Confirm corrosion exposure, forming and joining requirements before specifying it.

SELECTION NOTE

Do not treat it as a drop-in 304 substitute

430 belongs to the ferritic family, while 304 and 316L are austenitic. Check the service environment, fabrication route and required product standard before comparing or substituting grades.

MATERIAL RECORD

External references

4 cited sources

These sources support the short reference above. Use the contractual product standard, current mill documentation and service conditions for engineering and purchasing decisions.

  1. OutokumpuManufacturer dataModa ferritic stainless steel range
  2. British Stainless Steel AssociationIndustry association50 Grades of Stainless Steel
  3. British Stainless Steel AssociationDesignation referenceDuplex Stainless Steels: A Simplified Guide
  4. WikipediaBackground referenceSteel grades

Continue through the grade index